Dirt or Seediness

Dirt or Seediness

Dirt or Seediness Dust and dirt particles settle on the surface, during the application of the paint, the condition is called Dirt or Seediness. Possible Causes Solutions Unclean conditions in the surrounding area. Ensure that the painting area is clean. Dust in the...
Excessive Material Usage

Excessive Material Usage

Excessive Material Usage When the spray gun is not held as per the recommended guidelines, defects begin to appear. These defects are a direct result of Excessive Material Usage Possible Causes Solutions Failing to Trigger the gun at each stroke • Release the trigger...
Excessive Spray – Fog/Dry

Excessive Spray – Fog/Dry

Excessive Spray – Fog/Dry When the spray gun ejects excessive paint not as per recommended guidelines, defects appear. They are a direct consequence of Excessive Spray. Possible Causes Solutions Using Wrong Solvent blend Choose a slow evaporating thinner. Atomizing...
Orange Peel

Orange Peel

Orange Peel When the coated surface develops a kind of finish that resembles an orange peel, the defect is termed Orange Peel. The coating is not smooth but exhibits the texture of an orange. Possible Causes Solutions Improper Thinning of paint • Choose solvents that...
Sagging

Sagging

Sagging When the paint gives a downward drooping appearance, the condition is referred to as Sagging. This results when a heavier coat of paint is sprayed on a vertical, or a near vertical surface than the viscosity of the finish. Possible Causes Solutions Slow Over-...